Cited 4 times in

Comparison of Self-Etching Ceramic Primer and Conventional Silanization to Bond Strength in Cementation of Fiber Reinforced Composite Post

DC Field Value Language
dc.contributor.author노병덕-
dc.contributor.author방난심-
dc.contributor.author신유석-
dc.contributor.author정복영-
dc.date.accessioned2019-07-11T03:12:25Z-
dc.date.available2019-07-11T03:12:25Z-
dc.date.issued2019-
dc.identifier.urihttps://ir.ymlib.yonsei.ac.kr/handle/22282913/169876-
dc.description.abstractVarious mechanical and chemical surface treatments have been proposed to improve the retention of fiber-reinforced composite post (FRCP), but the results are still controversial. The bond strength and durability of a self-etching ceramic primer, which was recently released as an alternative to etching and silane, are not yet known. This study aimed to compare and evaluate the push-out bond strength of different surface treatments of FRCPs after an artificial aging procedure. Four groups (n = 10) were established to evaluated FRCP surface treatments (dentin adhesive bonding; silane and adhesive bonding; hydrofluoric acid, silane and adhesive bonding; and a self-etching ceramic primer). They were bonded with dual-curing rein cement (Multilink N) and stored in distilled water at 37 °C for 30 days, then thermal cycled for 7500 cycles. After being sectioned into 1 mm thickness, each coronal and apical part was evaluated for its the push-out bond strength by a universal testing machine. Each debonded specimen was observed by an optical microscope and divided according to the failure modes. The results showed that silane treatment significantly improved push-out bond strength, but the self-etching ceramic primer did not do so. Additional hydrofluoric acid treatment or the adhesive bonding agent alone did not significantly improve the retention of FRCPs. Cohesive failure of the luting material was found most frequently in all groups.-
dc.description.statementOfResponsibilityopen-
dc.languageEnglish-
dc.publisherMDPI-
dc.relation.isPartOfMATERIALS-
dc.rightsCC BY-NC-ND 2.0 KR-
dc.rightshttps://creativecommons.org/licenses/by-nc-nd/2.0/kr/-
dc.titleComparison of Self-Etching Ceramic Primer and Conventional Silanization to Bond Strength in Cementation of Fiber Reinforced Composite Post-
dc.typeArticle-
dc.contributor.collegeCollege of Dentistry (치과대학)-
dc.contributor.departmentDept. of Conservative Dentistry (보존과학교실)-
dc.contributor.googleauthorNan-Sim Pang-
dc.contributor.googleauthorBock-Young Jung-
dc.contributor.googleauthorByoung-Duck Roh-
dc.contributor.googleauthorYooseok Shin-
dc.identifier.doi10.3390/ma12101585-
dc.contributor.localIdA01280-
dc.contributor.localIdA01783-
dc.contributor.localIdA02129-
dc.contributor.localIdA03610-
dc.relation.journalcodeJ02182-
dc.identifier.eissn1996-1944-
dc.identifier.pmid31096562-
dc.subject.keywordFRC post-
dc.subject.keywordSelf-etching ceramic primer-
dc.subject.keywordpush-out bond strength-
dc.subject.keywordsurface treatment-
dc.contributor.alternativeNameRoh, Byoung Duck-
dc.contributor.affiliatedAuthor노병덕-
dc.contributor.affiliatedAuthor방난심-
dc.contributor.affiliatedAuthor신유석-
dc.contributor.affiliatedAuthor정복영-
dc.citation.volume12-
dc.citation.number10-
dc.citation.startPageE1585-
dc.identifier.bibliographicCitationMATERIALS, Vol.12(10) : E1585, 2019-
dc.identifier.rimsid62005-
dc.type.rimsART-
Appears in Collections:
2. College of Dentistry (치과대학) > Dept. of Advanced General Dentistry (통합치의학과) > 1. Journal Papers
2. College of Dentistry (치과대학) > Dept. of Conservative Dentistry (보존과학교실) > 1. Journal Papers

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.