483 712

Cited 19 times in

Debonding force and shear bond strength of an array of CAD/CAM-based customized orthodontic brackets, placed by indirect bonding- An In Vitro study.

Authors
 Ha-Na Sha  ;  Sung-Hwan Choi  ;  Hyung-Seog Yu  ;  Chung-Ju Hwang  ;  Jung-Yul Cha  ;  Kwang-Mahn Kim 
Citation
 PLOS ONE, Vol.13(9) : e0202952, 2018 
Journal Title
PLOS ONE
Issue Date
2018
Abstract
Based on three-dimensional scanning and computer-aided design and computer-aided manufacturing (CAD/CAM) techniques, customized bracket systems are increasingly used. However, data remain limited regarding customized bracket design, characteristics, and stability. This study was undertaken to evaluate the design, bond strength, and residual adhesives of four different CAD/CAM customized brackets that were attached to human tooth specimens by indirect bonding. Thirty extracted human upper premolars were divided into five groups: Group 1, preadjusted self-ligating labial metal bracket; Group 2, lingual self-ligating metal injection molding customized bracket; Group 3, gold-casted lingual customized bracket; Group 4, labial self-ligating milled customized bracket; Group 5, labial customized resin base bracket. Except in Group 1, premolar specimens were scanned via model scanner, and the images were sent to each manufacturing company to fabricate customized brackets and transfer trays/jigs. Debonding force (DF; N) was measured by Instron universal testing machine and shear bond strength (SBS; MPa) was calculated via dividing DF by bonding area. Adhesive remnants were analyzed via stereo microscopic images. Group 2 (196.90±82.75 N) exhibited significantly higher DF than Group 1 (62.77±12.65 N); other groups exhibited similar DFs, compared with Group 1. No customized bracket groups exhibited significant differences in SBS, relative to Group 1 (6.73±1.36 MPa). However, SBS in Group 5 (11.46±7.22 MPa) was significantly higher than in Group 3 (3.58±2.14 MPa). Group 3 had significantly lower ARI scores than other groups (P<0.05). Customized brackets exhibited large deviations in DF and SBS; all customized bracket systems exhibited DF that was equivalent or superior to that of preadjusted brackets, even when placed by indirect bonding
Files in This Item:
T201803652.pdf Download
DOI
10.1371/journal.pone.0202952
Appears in Collections:
2. College of Dentistry (치과대학) > Dept. of Dental Biomaterials and Bioengineering (치과생체재료공학교실) > 1. Journal Papers
2. College of Dentistry (치과대학) > Dept. of Orthodontics (교정과학교실) > 1. Journal Papers
Yonsei Authors
Kim, Kwang Mahn(김광만) ORCID logo https://orcid.org/0000-0002-5235-0294
Yu, Hyung Seog(유형석) ORCID logo https://orcid.org/0000-0002-1275-5078
Cha, Jung Yul(차정열)
Choi, Sung Hwan(최성환) ORCID logo https://orcid.org/0000-0002-1150-0268
Hwang, Chung Ju(황충주) ORCID logo https://orcid.org/0000-0003-3024-4551
URI
https://ir.ymlib.yonsei.ac.kr/handle/22282913/165222
사서에게 알리기
  feedback

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

Browse

Links