dc.description.abstract | INTRODUCTION: The aim of this study was to evaluate the micromorphologic changes that accompany different surface treatments on mineral trioxide aggregate (MTA) and their effect on the bond strength to the composite resin with 4 adhesive systems. METHODS: Three types of MTA cement, ProRoot MTA (WMTA) (Dentsply, Tulsa, OK), MTA Angelus (AMTA) (Angelus, Londrina, PR, Brazil), and Endocem MTA (EMTA) (Maruchi, Wonju, Korea), were prepared and stored for a week to encourage setting. Surface treatment was performed using phosphoric acid or self-etch primer, and an untreated MTA surface was prepared as a control. The surface changes were observed using scanning electron microscopy. MTA surfaces were bonded with 4 adhesive systems, including Scotchbond Multipurpose (3M ESPE, St Paul, MN), Single Bond 2 (3M ESPE), Clearfil SE BOND (Kuraray, Osaka, Japan), and AdheSE One F (Ivoclar Vivadent, Schaan, Liechtenstein), to evaluate the adhesive effectiveness of MTA followed by composite resin restoration. The shear bond strength of the polymerized specimens was tested. RESULTS: For WMTA and AMTA, untreated surfaces showed an irregular crystalline plate with clusters of globular aggregate particles. For EMTA, the untreated surface presented a reticular matrix with acicular crystals. After surface treatment, superficial crystalline structures were eroded regardless of the MTA cement and adhesive system used. WMTA bonded significantly more strongly than AMTA and EMTA, regardless of the adhesive system used. In the WMTA and AMTA groups, AdheSE One F showed the highest bond strength to the composite. For EMTA, no significant differences were found across adhesive systems. CONCLUSIONS: Acidic treatment of the MTA surface affected the micromorphology and the bond strength to the composite. Within the limitations of this study, using a 1-step self-etch adhesive system might result in a strong bond to WMTA when the composite resin restoration is required over MTA cement. | - |
dc.description.statementOfResponsibility | open | - |
dc.format.extent | 1210~1216 | - |
dc.relation.isPartOf | JOURNAL OF ENDODONTICS | - |
dc.rights | CC BY-NC-ND 2.0 KR | - |
dc.rights.uri | https://creativecommons.org/licenses/by-nc-nd/2.0/kr/ | - |
dc.subject.MESH | Acid Etching, Dental/methods | - |
dc.subject.MESH | Acrylic Resins/chemistry | - |
dc.subject.MESH | Aluminum Compounds/chemistry* | - |
dc.subject.MESH | Bismuth/chemistry | - |
dc.subject.MESH | Calcium Compounds/chemistry* | - |
dc.subject.MESH | Composite Resins/chemistry* | - |
dc.subject.MESH | Dental Bonding* | - |
dc.subject.MESH | Dental Cements/chemistry | - |
dc.subject.MESH | Dental Materials/chemistry* | - |
dc.subject.MESH | Dentin-Bonding Agents/chemistry | - |
dc.subject.MESH | Drug Combinations | - |
dc.subject.MESH | Humans | - |
dc.subject.MESH | Materials Testing | - |
dc.subject.MESH | Microscopy, Electron, Scanning | - |
dc.subject.MESH | Oxides/chemistry* | - |
dc.subject.MESH | Phosphoric Acids/chemistry | - |
dc.subject.MESH | Polymerization | - |
dc.subject.MESH | Random Allocation | - |
dc.subject.MESH | Resin Cements/chemistry | - |
dc.subject.MESH | Root Canal Filling Materials/chemistry* | - |
dc.subject.MESH | Shear Strength | - |
dc.subject.MESH | Silicates/chemistry* | - |
dc.subject.MESH | Stress, Mechanical | - |
dc.subject.MESH | Surface Properties | - |
dc.subject.MESH | Time Factors | - |
dc.title | Effect of mineral trioxide aggregate surface treatments on morphology and bond strength to composite resin | - |
dc.type | Article | - |
dc.contributor.college | College of Dentistry (치과대학) | - |
dc.contributor.department | Dept. of Conservative Dentistry (보존과학) | - |
dc.contributor.googleauthor | Shin Joo-Hee | - |
dc.contributor.googleauthor | Jang Ji-Hyun | - |
dc.contributor.googleauthor | Park Sang Hyuk | - |
dc.contributor.googleauthor | Kim Euiseong | - |
dc.identifier.doi | 10.1016/j.joen.2014.01.027 | - |
dc.admin.author | false | - |
dc.admin.mapping | false | - |
dc.contributor.localId | A00833 | - |
dc.relation.journalcode | J01393 | - |
dc.identifier.eissn | 1878-3554 | - |
dc.identifier.pmid | 25069935 | - |
dc.identifier.url | http://www.sciencedirect.com/science/article/pii/S0099239914000880 | - |
dc.subject.keyword | Adhesive system | - |
dc.subject.keyword | mineral trioxide aggregate | - |
dc.subject.keyword | scanning electron microscopy | - |
dc.subject.keyword | self-etch adhesive | - |
dc.contributor.alternativeName | Kim, Eui Seong | - |
dc.contributor.affiliatedAuthor | Kim, Eui Seong | - |
dc.rights.accessRights | free | - |
dc.citation.volume | 40 | - |
dc.citation.number | 8 | - |
dc.citation.startPage | 1210 | - |
dc.citation.endPage | 1216 | - |
dc.identifier.bibliographicCitation | JOURNAL OF ENDODONTICS, Vol.40(8) : 1210-1216, 2014 | - |
dc.identifier.rimsid | 57244 | - |
dc.type.rims | ART | - |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.