A new manufacturing method of all ceramic restoration using alumina tape and presentation of clinical cases

DC Field Value Language
dc.contributor.author김의성-
dc.contributor.author이근우-
dc.date.accessioned2019-11-11T06:10:55Z-
dc.date.available2019-11-11T06:10:55Z-
dc.date.issued2000-
dc.identifier.issn0301-2875-
dc.identifier.urihttps://ir.ymlib.yonsei.ac.kr/handle/22282913/172370-
dc.description.abstractIn an effort to facilitate fabrication procedure of all ceramic crowns, a novel preparation method for all ceramic crown using alumina tape was developed. The alumina tape having a uniform thickness was cast by using Doctor blade method. The physical properties of newly introduced alumina tape has biaxial flexure strength of 500.600 MPa. The value of toughness is 3.18~3,28 MPa.m(1/2) which corelates with facture and the linear shrinkage rate of the alumina tape is 0.44% during core production. The marginal fitness of the alumina tape all-ceramic restoration with 90degrees shoulder margin had average marginal discrepancy at 78.3micrometer and average marginal gap at 44.4micrometer. At the marginal preparation of 135degrees deep chamfer, the average marginal discrepancy at 82.1micrometer and the average marginal gap at 40.2micrometer had been reported. This fabrication procedure of all ceramic crowns with alumina tapes is easier and less technical sensitive for dental technicians. After restoration with new all ceramic crowns we followed the patients 2 years later, there were no complications as porcelain fractures or periodontal disease. We had good esthetic clinical results with new all ceramic crowns.-
dc.description.statementOfResponsibilityopen-
dc.languageKorean, English-
dc.publisherKorean Academy of Prosthodontics)-
dc.relation.isPartOfJournal of Korean Academy of Prosthodontics (대한치과보철학회지)-
dc.rightsCC BY-NC-ND 2.0 KR-
dc.titleA new manufacturing method of all ceramic restoration using alumina tape and presentation of clinical cases-
dc.typeArticle-
dc.contributor.collegeCollege of Dentistry (치과대학)-
dc.contributor.departmentDept. of Conservative Dentistry (보존과학교실)-
dc.contributor.googleauthorNam-Sik Oh-
dc.contributor.googleauthorEui-Seong Kim-
dc.contributor.googleauthorKeun-Woo Lee-
dc.contributor.googleauthorJung-Suk Han-
dc.contributor.googleauthorDae-Joon Kim-
dc.contributor.googleauthorMyung-Hyun Lee-
dc.contributor.localIdA00833-
dc.contributor.localIdA02688-
dc.relation.journalcodeJ01493-
dc.identifier.eissn2005-3789-
dc.subject.keywordAll ceramic crown-
dc.subject.keywordalumina tape-
dc.subject.keywordflexure strength-
dc.subject.keywordfithess-
dc.contributor.alternativeNameKim, Eui Seong-
dc.contributor.affiliatedAuthor김의성-
dc.contributor.affiliatedAuthor이근우-
dc.citation.volume38-
dc.citation.number6-
dc.citation.startPage800-
dc.citation.endPage805-
dc.identifier.bibliographicCitationJournal of Korean Academy of Prosthodontics (대한치과보철학회지), Vol.38(6) : 800-805, 2000-
Appears in Collections:
2. College of Dentistry (치과대학) > Dept. of Conservative Dentistry (보존과학교실) > 1. Journal Papers
2. College of Dentistry (치과대학) > Dept. of Prosthodontics (보철과학교실) > 1. Journal Papers

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.