Cited 13 times in
The effect of different cooling rates and coping thicknesses on the failure load of zirconia-ceramic crowns after fatigue loading
DC Field | Value | Language |
---|---|---|
dc.contributor.author | 김선재 | - |
dc.contributor.author | 김지환 | - |
dc.contributor.author | 심준성 | - |
dc.date.accessioned | 2018-07-20T08:11:44Z | - |
dc.date.available | 2018-07-20T08:11:44Z | - |
dc.date.issued | 2017 | - |
dc.identifier.issn | 2005-7806 | - |
dc.identifier.uri | https://ir.ymlib.yonsei.ac.kr/handle/22282913/160947 | - |
dc.description.abstract | PURPOSE: The purpose of this study was to evaluate the influence of different coping thicknesses and veneer ceramic cooling rates on the failure load of zirconia-ceramic crowns. MATERIALS AND METHODS: Zirconia copings of two different thicknesses (0.5 mm or 1.5 mm; n=20 each) were fabricated from scanning 40 identical abutment models using a dental computer-aided design and computer-aided manufacturing system. Zirconia-ceramic crowns were completed by veneering feldspathic ceramics under different cooling rates (conventional or slow, n=20 each), resulting in 4 different groups (CONV05, SLOW05, CONV15, SLOW15; n=10 per group). Each crown was cemented on the abutment. 300,000 cycles of a 50-N load and thermocycling were applied on the crown, and then, a monotonic load was applied on each crown until failure. The mean failure loads were evaluated with two-way analysis of variance (P=.05). RESULTS: No cohesive or adhesive failure was observed after fatigue loading with thermocycling. Among the 4 groups, SLOW15 group (slow cooling and 1.5 mm chipping thickness) resulted in a significantly greater mean failure load than the other groups (P<.001). Coping fractures were only observed in SLOW15 group. CONCLUSION: The failure load of zirconia-ceramic crowns was significantly influenced by cooling rate as well as coping thickness. Under conventional cooling conditions, the mean failure load was not influenced by the coping thickness; however, under slow cooling conditions, the mean failure load was significantly influenced by the coping thickness. | - |
dc.description.statementOfResponsibility | open | - |
dc.language | English | - |
dc.publisher | Korean Academy of Prosthodontics | - |
dc.relation.isPartOf | JOURNAL OF ADVANCED PROSTHODONTICS | - |
dc.rights | CC BY-NC-ND 2.0 KR | - |
dc.rights | https://creativecommons.org/licenses/by-nc-nd/2.0/kr/ | - |
dc.title | The effect of different cooling rates and coping thicknesses on the failure load of zirconia-ceramic crowns after fatigue loading | - |
dc.type | Article | - |
dc.contributor.college | College of Dentistry | - |
dc.contributor.department | Dept. of Prosthodontics | - |
dc.contributor.googleauthor | Yu Lung Tang | - |
dc.contributor.googleauthor | Jee-Hwan Kim | - |
dc.contributor.googleauthor | June-Sung Shim | - |
dc.contributor.googleauthor | Sunjai Kim | - |
dc.identifier.doi | 10.4047/jap.2017.9.3.152 | - |
dc.contributor.localId | A00558 | - |
dc.contributor.localId | A01006 | - |
dc.contributor.localId | A02211 | - |
dc.relation.journalcode | J01223 | - |
dc.identifier.eissn | 2005-7814 | - |
dc.identifier.pmid | 28680545 | - |
dc.subject.keyword | Cooling rate | - |
dc.subject.keyword | Coping thickness | - |
dc.subject.keyword | Failure | - |
dc.subject.keyword | Zirconia | - |
dc.contributor.alternativeName | Kim, Sun Jai | - |
dc.contributor.alternativeName | Kim, Jee Hwan | - |
dc.contributor.alternativeName | Shim, June Sung | - |
dc.contributor.affiliatedAuthor | Kim, Sun Jai | - |
dc.contributor.affiliatedAuthor | Kim, Jee Hwan | - |
dc.contributor.affiliatedAuthor | Shim, June Sung | - |
dc.citation.volume | 9 | - |
dc.citation.number | 3 | - |
dc.citation.startPage | 152 | - |
dc.citation.endPage | 158 | - |
dc.identifier.bibliographicCitation | JOURNAL OF ADVANCED PROSTHODONTICS, Vol.9(3) : 152-158, 2017 | - |
dc.identifier.rimsid | 60841 | - |
dc.type.rims | ART | - |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.